TECHNET Archives

February 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Steve Gregory <[log in to unmask]>
Date:
Tue, 28 Feb 2017 22:51:16 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Nutting, Phil" <[log in to unmask]>
Message-ID:
Content-Transfer-Encoding:
base64
Subject:
From:
"Nutting, Phil" <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Steve,



It was a Shercon product, but not the ones you listed.



Phil



From: Steve Gregory [mailto:[log in to unmask]]

Sent: Tuesday, February 28, 2017 4:58 PM

To: Nutting, Phil

Cc: TechNet E-Mail Forum

Subject: Re: [TN] Baking before conformal coating



Hi Phil,

We've been using Shercon KD Kwiky Dot Discs which are supposed to have an acrylic adhesive:



http://www.all-spec.com/Catalog/Adhesives-Sealants-Tapes/Tapes/Dots-Discs/KD00312-45075

Those aren't the ones you are using are they?

Steve



On Tue, Feb 28, 2017 at 2:35 PM, Nutting, Phil <[log in to unmask]<mailto:[log in to unmask]>> wrote:

With our acrylic conformal coating I noticed a blooming effect around the masking tape dots.  It turned out that the tape dots had changed from acrylic adhesive to silicon adhesive.



Phil



-----Original Message-----

From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Steve Gregory

Sent: Tuesday, February 28, 2017 4:19 PM

To: [log in to unmask]<mailto:[log in to unmask]>

Subject: Re: [TN] Baking before conformal coating



I don't know what the heck is going on here, but try these links!



Arrrrrrrrrgh!



http://stevezeva.homestead.com/Conformal_dark_spots.jpg



http://stevezeva.homestead.com/Conformal_dark_spots_close.jpg



http://stevezeva.homestead.com/Conformal_dark_spots_close_reflected_light.jpg



Steve



On Tue, Feb 28, 2017 at 2:14 PM, Steve Gregory <[log in to unmask]<mailto:[log in to unmask]>> wrote:



> Oh shoot, I sent thumbnail links! Here try these:

>

> http://stevezeva.homestead.com/Conformal_dark_spots.jpg

> <http://stevezeva.homestead.com/Conformal_dark_spots_thumb.jpg>

>

> http://stevezeva.homestead.com/Conformal_dark_spots_close.jpg

> <http://stevezeva.homestead.com/Conformal_dark_spots_close_thumb.jpg>

>

> http://stevezeva.homestead.com/Conformal_dark_spots_close_

> reflected_light.jpg

> <http://stevezeva.homestead.com/Conformal_dark_spots_close_reflected_light_thumb.jpg>

>

>

> Steve

>

>

> On Tue, Feb 28, 2017 at 2:07 PM, Steve Gregory <[log in to unmask]<mailto:[log in to unmask]>> wrote:

>

>> Hi Doug, Lloyd and everyone,

>>

>> Here are some photos:

>>

>> Area under UV light (BTW, that's my Ray-O-Vac pet pee-pee detector light

>> I bought at Walmart):

>>

>> http://stevezeva.homestead.com/Conformal_dark_spots_thumb.jpg

>>

>> Close-up of area under UV light:

>>

>> http://stevezeva.homestead.com/Conformal_dark_spots_close_thumb.jpg

>>

>> Close-up of the same area under reflected light:

>>

>> http://stevezeva.homestead.com/Conformal_dark_spots_close_

>> reflected_light_thumb.jpg

>>

>> So you can see that the area is indeed coated. This is Humiseal 1B73....

>>

>> Steve

>>

>> On Tue, Feb 28, 2017 at 1:51 PM, Douglas Pauls <

>> [log in to unmask]<mailto:[log in to unmask]>> wrote:

>>

>>> Argggh Steve, we know ye to be a pirate anyways......

>>>

>>> I had the same question come to mind as Lloyd asked.  Pinholes or

>>> dewetting?  Pinholes can be due to moisture coming out of the board, but is

>>> most often point sources of contamination, like droplets of oil or some

>>> other adulterating contaminant in the coating.  A picture would help.

>>>

>>>

>>> Doug Pauls

>>> Principal Materials and Process Engineer

>>> Rockwell Collins

>>>

>>> On Tue, Feb 28, 2017 at 2:20 PM, Steve Gregory <[log in to unmask]<mailto:[log in to unmask]>>

>>> wrote:

>>>

>>>> Hi all,

>>>>

>>>> I'm not trying to hijack this thread, but since we're talking conformal

>>>> coating here, what could cause an acrylic to appear that there are tiny

>>>> little fisheyes in the coating, but when you hold the board at an angle,

>>>> you can clearly see that the area is coated. I know pictures would help,

>>>> I'll see if I can get some....

>>>>

>>>> Steve

>>>>

>>>> On Tue, Feb 28, 2017 at 12:59 PM, lduso - Diamond-MT.com <

>>>> [log in to unmask]<mailto:[log in to unmask]>> wrote:

>>>>

>>>> > We do not pre-bake as an internal rule and never a complaint. Obvious

>>>> > exceptions: We are washing or cleanliness testing the boards. Then we

>>>> will

>>>> > bake them dry before masking and coating. Or the customer specifically

>>>> > requires a pre-bake on the drawing. (I always then ask the question;

>>>> "How

>>>> > long after the bake do I have to coat them before they need to be

>>>> baked

>>>> > again?" Strangely, only a few have an answer for that.)

>>>> >

>>>> > I have visited many facilities that conformal coat and I have

>>>> witnessed it

>>>> > both ways but mostly on the "no pre-bake" side. One customer even

>>>> pre-baked

>>>> > their boards before coating with a water based acrylic.

>>>> >

>>>> > Lloyd Duso

>>>> > Plant Manager

>>>> > Diamond-MT

>>>> > (814) 535-3505<tel:%28814%29%20535-3505>

>>>> > www.Diamond-mt.com<http://www.Diamond-mt.com>

>>>> >

>>>> > On Tue, Feb 28, 2017 at 2:39 PM, Douglas Pauls <

>>>> > [log in to unmask]<mailto:[log in to unmask]>> wrote:

>>>> >

>>>> > > Lee,

>>>> > > It Depends.

>>>> > >

>>>> > > We have one facility that has never baked prior to coating

>>>> application.

>>>> > No

>>>> > > evidence of any conformal coating related problems.  We have several

>>>> > > facilities that bake religiously prior to coating application, also

>>>> for

>>>> > > acrylic.  No evidence of any conformal coating related problems.

>>>> > >

>>>> > > I think the biggest factor is how much residual water you have.  I

>>>> don't

>>>> > > think your assemblies have to be bone dry before coating.  We do a

>>>> lot

>>>> > with

>>>> > > in-line aqueous cleaners, which have heated air knifes that remove

>>>> the

>>>> > bulk

>>>> > > of the water.  Now, there might still be some entrapment areas, but

>>>> if

>>>> > so,

>>>> > > we find them and then blow out those entrapment areas with ionized

>>>> air.

>>>> > >

>>>> > >

>>>> > > Doug Pauls

>>>> > > Principal Materials and Process Engineer

>>>> > > Rockwell Collins

>>>> > >

>>>> > > On Tue, Feb 28, 2017 at 10:20 AM, Lee Hitchens <

>>>> > > [log in to unmask]<mailto:[log in to unmask]>

>>>> > > > wrote:

>>>> > >

>>>> > > > Hi all

>>>> > > >

>>>> > > > I've recently been asked about baking pcbs before conformal

>>>> coating and

>>>> > > > whether there is any quantified data on the effect on coating

>>>> > > performance.

>>>> > > >

>>>> > > > Does anyone know of any public studies on this or can shed some

>>>> light

>>>> > on

>>>> > > > its effectiveness beyond anecdotal experience ? I would be very

>>>> > grateful

>>>> > > to

>>>> > > > you on this.

>>>> > > >

>>>> > > > Best Regards

>>>> > > >

>>>> > > > Dr Lee Hitchens

>>>> > > >

>>>> > > > SCH Technologies is a Division of SCH Services Limited

>>>> > > >

>>>> > > > www.conformalcoating.co.uk<http://www.conformalcoating.co.uk>

>>>> > > > Skype: leehitchens

>>>> > > >

>>>> > >

>>>> >

>>>>

>>>> --

>>>>

>>>>

>>>> This email and any attachments are only for use by the intended

>>>> recipient(s) and may contain legally privileged, confidential,

>>>> proprietary

>>>> or otherwise private information. Any unauthorized use, reproduction,

>>>> dissemination, distribution or other disclosure of the contents of this

>>>> e-mail or its attachments is strictly prohibited. If you have received

>>>> this

>>>> email in error, please notify the sender immediately and delete the

>>>> original.

>>>>

>>>

>>>

>>

>



--





This email and any attachments are only for use by the intended

recipient(s) and may contain legally privileged, confidential, proprietary

or otherwise private information. Any unauthorized use, reproduction,

dissemination, distribution or other disclosure of the contents of this

e-mail or its attachments is strictly prohibited. If you have received this

email in error, please notify the sender immediately and delete the

original.





[Image removed by sender.]



This email and any attachments are only for use by the intended recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.


ATOM RSS1 RSS2