Another example of why I try never to use ENIG plating if at all
possible.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Wednesday, September 20, 2006 11:54 AM
To: [log in to unmask]
Subject: Re: [TN] ENIG Problem...
Probably related Steve.
If the pads look like copper, then it is either a total skip plate OR it
has skipped nickel and the gold plate has dissolved into the copper.
If you have some bare boards showing the issue it is a relatively simple
task to get the board vendor to confirm with XRF.
On a reliability issue I would say yes you are pretty much hosed.
John
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, September 20, 2006 8:48 AM
To: [log in to unmask]
Subject: [TN] ENIG Problem...
Hi All!
Wouldn't you know it, all these postings about ENIG and all of a sudden
an issue just started happening with some ENIG boards we're building.
The problem is sporadic. We're building a double-sided SMT board using a
SAC 305 paste, and I haven't seen any non-wetting problems with the SMT
yet.
We're selective wave soldering using SN96 and a RMA flux, and after
about 250-300 boards my touch-up operators flagged me down and said that
they're seeing some boards that have through-hole pads that aren't
wetting no matter what they do. Here's some pictures:
http://stevezeva.homestead.com/files/Non_Wetting_Pads.jpg
http://stevezeva.homestead.com/files/Non_Wetting_Pads_2.jpg
http://stevezeva.homestead.com/files/Non_Wetting_Pads_Close.jpg
The pads look like bare copper...no nickle. Is this related to the
latest thread? Like I said I haven't seen any SMT with this issue (yet),
and it just started showing up...we've built a few hundred boards with
no problems until now.
I'm having the operators set the boards aside with the problem. Am I
pretty much hosed with these boards?
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|