Solder pot purity maintenance is specified in J-STD-001. Copper limit is
0.300% The J-STD-006 is a specification for electronic grade solder alloy.
This is what you should get when you purchase fresh solder.
Guy Ramsey
American Competitiveness Institute
Senior Lab Technician / Instructor
610 362-1200 ext 107
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Susan James
Sent: Wednesday, February 28, 2001 1:07 PM
To: [log in to unmask]
Subject: [TN] Copper levels in wave solder pot
Gurus,
After having our solder pot analyzed, the copper level is showing .1273.
In July of 1999, the copper level was .120. We are assuming the copper is
coming from the cut component leads. My concern is whether or not this is
significant enough to change out the solder. J-STD-006 specs .08 as
acceptable but I don't know how "bad" .1273 is considered to be. Any help
is appreciated.
Sue James
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|