TECHNET Archives

March 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Date:
Thu, 21 Mar 2002 08:25:53 +0800
Content-type:
text/plain; charset=us-ascii
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Juan Li <[log in to unmask]>
Parts/Attachments:
text/plain (24 lines)
As the circuitry width become finer (3/3 mil, 2.5/2.5mil), I would like to know
whether the line width tolerance got new specification or not.
For PCB, the general IPC standard is 20% of circuitry width.  Let's say
circuitry width 6mil got +30um tolerance.  If circuitry width 3mil, do we still
use 20% of circuitry width as the specification.  Does IPC have the new
specification for fine lines?  Or from the PCB design point of view, what should
be the general tolerance for 3/3mil and 2.5/2.5mil?

Wish your helpful information!

Best regards!
Li Juan

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2