Joe,
What type of cleaner do you have? Does it have a standard 2 blower drying with IR assist or other? What is the dwell time within the dryer module(s) within the washer? We do what you are describing and have had no issues to speak of, but we do have a good washer with excellent drying capacity... Please describe your wash process...
CAS
Chris Schaefer
Suntron Corporation
Process Engineer
540 N. Rogers Road
Olathe, Kansas 66062
913.393.5878
[log in to unmask]
NOTICE:
This message is intended for the use of the individual entity to which it is addressed and may contain information that is privileged, confidential and exempt from disclosure under applicable law. If the reader of this message is not the intended recipient, or the employee or agent responsible for delivering the message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by calling 913.393.5878 or returning the original message to us.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Macko, Joe @ IEC
Sent: Wednesday, September 06, 2006 11:31 AM
To: [log in to unmask]
Subject: [TN] Populated board bake out after 1st side reflow/DI wash
Fellow techs,
Hello.
A general question came up about the need to re-bake a double sided board
after 1st side reflow/DI wash before starting 2nd side assembly. The concern
is that the board (or mounted MSDs) may absorb enough moisture going through
the high-pressure DI water in-line cleaner to potentially cause a problem
during 2nd side reflow. There are some MSDs mounted on the 1st side but both
sides are assembled before exceeding any of the component's floor life. It
has been suggested that some level of bake out should be performed after 1st
side cleaning to prevent potential problems during 2nd side reflow but the
push back is that this adds cost, handling, etc... that may introduce its
own associated problems and is not really necessary.
Thanks again. It is great to have a knowledgeable forum such as TechNet.
Joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|