TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
Date:
Fri, 26 Oct 2001 11:26:21 -0500
Content-Type:
multipart/mixed; boundary="=_D48E3BD0.F293FE86"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (512 bytes) , TEXT.htm (867 bytes)
I dealt with this issue about two years ago.  Some of the voids we had found were quite large and exposed the internal circuitry but others were very small and didn't expose the internals.  We ended up making a size maximum which at that application was .020".  If the part had a void that was larger than that it was unacceptable but if it was smaller than that we allowed a small patch.  The application wasn't affected by patches.  We were more worried about entrappment through wave and wash.  

Kathy 



<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN"> <HTML><HEAD> <META content="text/html; charset=iso-8859-1" http-equiv=Content-Type> <META content="MSHTML 5.00.2919.6307" name=GENERATOR></HEAD> <BODY style="FONT: 10pt Abadi MT Condensed Light; MARGIN-LEFT: 2px; MARGIN-TOP: 2px"> <DIV>I dealt with this issue about two years ago.&nbsp; Some of the voids we had found were quite large and exposed the internal circuitry but others were very small and didn't expose the internals.&nbsp; We ended up making a size maximum which at that application was .020".&nbsp; If the part had a void that was larger than that it was unacceptable but if it was smaller than that we allowed a small patch.&nbsp; The application wasn't affected by patches.&nbsp; We were more worried about entrappment through wave and wash.&nbsp; </DIV> <DIV>&nbsp;</DIV> <DIV>Kathy </DIV></BODY></HTML>