Hi,
I have very successfully used Corona Discharge, a non vacuum form or
plasma, to clean parts and improve adhesive adhesion.
It creates a fair amount of Ozone while running.
Chuck
Charles W. Brummer | 3M Manufacturing Engineer
3M Electronic Solutions Division
3M Canoga Park, 8357 Canoga Ave. | Canoga Park, CA 91304
Office: 818 734 4930
[log in to unmask] | www.3M.com
This message (including any attachments) may contain material, non-public
information or proprietary information and is for the intended recipients
only. If you are not the intended recipient, you should notify the sender
and delete this message. Any disclosure, copying, or use of this
information is strictly prohibited and may subject you to legal liability.
From: "Neifer, Gebhard" <[log in to unmask]>
To: <[log in to unmask]>
Date: 11/14/2013 12:48 AM
Subject: [TN] AW: UV-Ozone Cleaning Processes
Sent by: TechNet <[log in to unmask]>
Rich,
as far as I know UV-Ozone is not capable to remove inorganic
contaminations. Plasma on the other hand can remove both, organic and
inorganic residues...
Gebhard
-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Richard Kraszewski
Gesendet: Mittwoch, 13. November 2013 18:08
An: [log in to unmask]
Betreff: [TN] UV-Ozone Cleaning Processes
Are any of you familiar with UV-Ozone cleaning processes? I am
considering using Plasma to clean some PCA's prior to coating to improve
wetting of coatings, but now wonder if I should also consider UV-Ozone.
Anyone care to state some pros and cons of each for my application?
Suprisingly enough, I don't see any mention of UV-Ozone cleaning in the
IPC -CH65B handbook.
Thanks
Rich Kraszewski / Plexus
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
****************************************************************************************
Note: If the reader of this message is not the intended recipient, or an
employee or agent responsible for delivering this message to the intended
recipient, you are hereby notified that any dissemination, distribution or
copying of this communication is strictly prohibited. If you have received
this communication in error, please notify us immediately by replying to
the message and deleting it from your computer. Thank you.
****************************************************************************************
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|