TECHNET Archives

August 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
Guenter Grossmann <[log in to unmask]>
Date:
Fri, 8 Aug 1997 11:54:44 +0200
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Guenter Grossmann <[log in to unmask]>
Parts/Attachments:
text/plain (21 lines)
Russ

When I was dealing with the problem of micro BGA's and FinePitch components
we found that HAL surfaces can be produced with a surface flat enough to
satisfy the needs of fine pitch production. However, the boards had to be
plated in a brand new horizontal HAL machine which was quite expensive. I
don't think this equipment will be standard in near future. We had no
problems with NiAu and OSP's. The easiest PCB to work with where those with
a Solid Solder Deposition (SSD) finish. They where already fluxed with a
slightly sticky flux. With these boards we went so several companies who
had no experience in using FinePitch components in every place we had no
troubles in the production of a lot of 50 pieces. Sure this test is non
representative for a large scale production. But I think it shows that SSD
could be a valuable alternative to other production processes when things
are getting tough.