TECHNET Archives

October 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Charles Caswell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 30 Oct 2003 16:22:15 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (47 lines)
Put it back in the fridge. Next time you use it dispense a little bit to clear the tip before using. I have done it this way with locktite SMT adhesive for years with no problems. 


-----Original Message-----
From: Peter L. [mailto:[log in to unmask]]
Sent: Thursday, October 30, 2003 3:29 PM
To: [log in to unmask]
Subject: [TN] SMT adhesive Handling


Technet,

Can anyone share their current procedure in handling left-over SMT adhesive
in the cartridge? What would be the preferred process for handling and
storage the adhesive for later uses?

We currently discard any left-over adhesive on the line after the build. As
for the unused adhesive remained in the cartridge, we were informed by the
supplier (Loctite) either to consume it within a max. of 10 days or return
it right back to the fridge. In that case I am concerned with the impact of
repeated refrigeration has on the adhesive shelve life.

Any feedback will be appreciated.

Rgds,
Peter

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2