Down load the Applications Note "Soldering to gold" from our website, it
says same as below but with the numbers, plus a bit more.

Regards

Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack C. Olson
Sent: Monday, December 06, 2004 4:31 PM
To: [log in to unmask]
Subject: Re: [TN] Gold Plated Board


The amount of gold on an "Immersion" plated board
is only a few microinches think, usually less than 10.
When you solder a component to that surface, some
or all of the gold (depending on how long the solder
stays heated/melted) mixes in with the solder joint.
If the percentage of gold in the solder joint is high
enough the joint will be brittle, but it won't be that
high with such a thin immersion finish.

Trying to solder to a thick electroplated gold surface
is a different story, however, but you can calculate it
yourself by comparing the thickness of gold plating
with the amount of solder paste you are applying to
the lands in question. I can't remember the exact
percentage that means you are getting into the "danger
zone", but someone here will know it, or you can search
the TechNet archives at:
http://listserv.ipc.org/archives/technet.html

good luck,
Jack

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


:::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2