TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 21 Jul 2009 15:10:56 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Subject:
From:
Graham Naisbitt <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<20090721084011.QIUL4.69292.root@ispmxfep13-z02>
Content-Type:
text/plain; charset="US-ASCII"; format=flowed; delsp=yes
MIME-Version:
1.0 (Apple Message framework v935.3)
Parts/Attachments:
text/plain (165 lines)
Dewey! - DEWEY!! - You have a challenger!

Graham Naisbitt

On 21 Jul 2009, at 14:40, Susy Webb wrote:

> Well we are called space city!!!!
>
> By the way, we take the shuttle to work where we design celestial PC  
> boards at our station using moon units (sorry Frank Zappa) so we  
> have space for everything. We eat moon pies while we make moola all  
> week until we crater on friday only to drink a little moonshine  
> until we fall asleep in the moonbeams... only to start it all again  
> on moonday!
>
> Sorry ... I couldn't resist. To those of you didn't care for the  
> interruption, I apologize and I will be quiet now!!!
>
>
> Susy
>
> ---- Inge <[log in to unmask]> wrote:
>> Do you have space for that?
>> /Inge
>>
>>
>> ----- Original Message -----
>> From: "Susy Webb" <[log in to unmask]>
>> To: <[log in to unmask]>
>> Sent: Tuesday, July 21, 2009 12:12 AM
>> Subject: Re: [TN] NTC:Moonshine?
>>
>>
>>> How do we in Houston celebrate today? Why by doing the "moon  
>>> walk", of
>>> course!
>>>
>>> Susy
>>>
>>>
>>> ----- Original Message -----
>>> From: "Barbara Burcham" <[log in to unmask]>
>>> To: <[log in to unmask]>
>>> Sent: Monday, July 20, 2009 4:36 PM
>>> Subject: Re: [TN] NTC:Moonshine?
>>>
>>>
>>>> How do we celebrate in Houston?
>>>> Any old way we want to.
>>>>
>>>> What are we celebrating?
>>>> Moon Landing?
>>>> Again, any way we want?
>>>> Barbara
>>>>
>>>> On Mon, Jul 20, 2009 at 3:11 PM, Inge <[log in to unmask]>  
>>>> wrote:
>>>>
>>>>> Well, how do they celebrate in Houston today? /Inge
>>>>>
>>>>> ---------------------------------------------------
>>>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>>>> To unsubscribe, send a message to [log in to unmask] with  
>>>>> following text
>>>>> in
>>>>> the BODY (NOT the subject field): SIGNOFF Technet
>>>>> To temporarily halt or (re-start) delivery of Technet send e- 
>>>>> mail to
>>>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>>> To receive ONE mailing per day of all the posts: send e-mail to
>>>>> [log in to unmask]: SET Technet Digest
>>>>> Search the archives of previous posts at:
>>>>> http://listserv.ipc.org/archives
>>>>> Please visit IPC web site
>>>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional
>>>>> information, or contact Keach Sasamori at
>>>>> [log in to unmask] or 847-615-7100 ext.2815
>>>>> -----------------------------------------------------
>>>>>
>>>>
>>>>
>>>>
>>>> -- 
>>>> Barbara Burcham, C.I.D.
>>>> pcb Trace Design
>>>> 281-341-7539 Wk/Hm
>>>> 713-249-7718 Cell
>>>> [log in to unmask]
>>>>
>>>> ---------------------------------------------------
>>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>>> To unsubscribe, send a message to [log in to unmask] with following  
>>>> text in
>>>> the BODY (NOT the subject field): SIGNOFF Technet
>>>> To temporarily halt or (re-start) delivery of Technet send e-mail  
>>>> to
>>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>> To receive ONE mailing per day of all the posts: send e-mail to
>>>> [log in to unmask]: SET Technet Digest
>>>> Search the archives of previous posts at:
>>>> http://listserv.ipc.org/archives
>>>> Please visit IPC web site
>>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>>> information, or contact Keach Sasamori at [log in to unmask] or  
>>>> 847-615-7100
>>>> ext.2815
>>>> -----------------------------------------------------
>>>
>>> ---------------------------------------------------
>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>> To unsubscribe, send a message to [log in to unmask] with following  
>>> text in
>>> the BODY (NOT the subject field): SIGNOFF Technet
>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>> To receive ONE mailing per day of all the posts: send e-mail to
>>> [log in to unmask]: SET Technet Digest
>>> Search the archives of previous posts at: http://listserv.ipc.org/archives
>>> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>> for additional information, or contact Keach Sasamori at [log in to unmask] 
>>>  or
>>> 847-615-7100 ext.2815
>>> -----------------------------------------------------
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following  
>> text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail  
>> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask] 
>> : SET Technet Digest
>> Search the archives of previous posts at: http://listserv.ipc.org/archives
>> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
>>  for additional information, or contact Keach Sasamori at [log in to unmask] 
>>  or 847-615-7100 ext.2815
>> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following  
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask] 
> : SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask] 
> : SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
>  for additional information, or contact Keach Sasamori at [log in to unmask] 
>  or 847-615-7100 ext.2815
> -----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2