Hi Ron,
Is the assembly to dense to "glue" the components down with a water soluble
mask?
Hans
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Process Engineer
Toppan Electronics, Inc.
770 Miramar Road
San Diego, CA 92126
(858) 695 - 2222 ext. 241
(858) 695 - 6823 fax
[log in to unmask]
-----Original Message-----
From: Mark Gilbert [mailto:[log in to unmask]]
Sent: Thursday, November 09, 2000 1:00 PM
To: [log in to unmask]
Subject: Re: [TN] Wave Soldering
Same here. I my previous life we used custom-made weighted fixtures we
designed in-house to hold several LEDs in place during a wave solder
process.
Regards,
Mark Gilbert, Product/Process Engineer
FOX Electronics
For Frequency Control Solutions. . . Fast:
1-888-GET2FOX, ext. 2289
Direct Phone# 1-941-690-2289
Fax: 941-693-1554
http://www.foxonline.com/
-----Original Message-----
From: Chad Haima [mailto:[log in to unmask]]
Sent: Thursday, November 09, 2000 3:39 PM
To: [log in to unmask]
Subject: Re: [TN] Wave Soldering
Ron,
I've had a few customers that have used sandbags and even hockey pucks but I
believe they made them themselves. I'm sure this is no help.
Regards,
Chad Haima
National Sales Manager
S.P. Precision Int'l
www.spprecision.com
503-357-9228
-----Original Message-----
From: Ron Waugh [mailto:[log in to unmask]]
Sent: Thursday, November 09, 2000 12:22 PM
To: [log in to unmask]
Subject: [TN] Wave Soldering
To All,
I have an assembly that has a few components that want to float while
going over the wave solder. In my past life we used sandbags, but as
the story goes I can't seem to remember where they were purchased. I
was wondering if anyone out there knew where I could get my hands on
some. Thank you in advance for your time and energy.
Regards,
Ron Waugh
Process Engineer
Diversified Systems, Inc.
Phone (317) 299-9547 Ext. 336
Fax (317) 298-2055
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|