Hi,
I would take a flex pcb, pure Polyimide as this is thin and nothing to outgas...
Best Regards,
Torsten
i.A. Dipl.Ing.(FH)Torsten Hagge
team leader HW development &
tech. projectmanager
Kristronics GmbH
Gewerbegrund 5 - 9
24955 Harrislee
Tel.: +49 461 7741 624
Fax: +49 461 7741 642
[log in to unmask]
www.kristronics.de
Gerichtsstand Flensburg, Handelsregister: HRB 1433 FL
Geschäftsführer Dipl.-Ing. oec. Thormod Ohm
Ust-Id-Nr. DE 811182059
Bankverbindung: Deutsche Bank AG Flensburg, Konto-Nr. 4216610, BLZ 21570011
IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215
-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Kenneth J. Wood
Gesendet: Freitag, 29. Juli 2011 15:52
An: [log in to unmask]
Betreff: [TN] High Vacuum Substrate
Hi all,
I have a PCB that operates inside a vacuum chamber under ultra high vacuum.
The material can't outgas and needs to hold up physically under the pressure (or lack thereof).
I wanted to use RO3003 but may need something else, any suggestions?
Material lead time is an issue as well which is why I'm looking...
Thanks
Ken
_____________________________________
Kenneth J. Wood
Saturn PCB Design, Inc.
www.saturnpcb.com
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|