We only remove small areas for individual component rework and then simply
burn through the material with a soldering iron as part of the unsoldering
step. We have never had the need to remove this type coating from an entire
board...that would essentially be destructive. We have removed all acrylic
coating though because it dissolves in IPA and also Acetone.
> Rainer G. Blomberg
> Honeywell -Space Systems Clearwater
> Staff Production Engineer
(727) 539-5534
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joseph H. Smith
Sent: Tuesday, December 13, 2005 9:48 AM
To: [log in to unmask]
Subject: [TN] Help with removing UR Conformal Coating
Has anyone had experience or success with removing conformal coating for PWA
that has been coated with UR coating especially using a chemical means. I
am particularly interested with how you handled coating around or under
BGA's.
Any help would be grateful.
Thanks.
Andrew Kettlewell
Process Engineer
Sypris Electronics
Tampa, FL
___________________________________________________
Try the New Netscape Mail Today!
Virtually Spam-Free | More Storage | Import Your Contact List
http://mail.netscape.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|