TECHNET Archives

August 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 30 Aug 2018 15:26:15 -0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Collins <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; charset=utf-8; format=flowed
From:
Graham Collins <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Hi technet!

We've got a customer working with high power transistors, they want to 
use solder pre-forms to solder a heatsink on top of a row of 
transistors.  So the stackup will be PCB - transistor - preform - 
heatsink, where the heatsink will span a row of 5 transistors.

The question is how do we establish that this is working OK and isn't 
full of voids?  This is at the "ok, we think this will work but we need 
to qualify the attachment method" stage.  I've come up with a couple of 
options:

1) tear / grind it off and look for anomalies - not very sure to find 
issues.
2) x-ray it - we don't have a 3-d x-ray so I'm not confident in our 
abilities to find voiding.  We do have a nice static x-ray though and 
will try it to see how well it can see.
3) Sonoscan it to look for voids?  Would have to be outsourced.

Am I missing any obvious options?

-- 