The best way to titrate weak acid is by back titration, using the suitable indicator.
You first add a known amount of a strong alkali and titrate the "overdose".
WHATEVER wrote:
> I wonder how many of you using acid stoper during developing of dry film?
> say citric acid. and I would like to hear your comments. For those chemists
> out there, I like to know whether it is really possible to titrate a weak
> acid with three Ka ?
>
> Oh, by the way, anyone using resist lamintor with two sets of rollers, hot
> to hot; Like to try or modify a one, if you have some information, would you
> please share with me?
>
> Thanks.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
--
Jacob Mozel
11 Hakalanit St
44280 Kfar Saba, Israel
Tel: +972 9 7425871
Fax: +972 9 7424089
e-mail: <[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|