Being said all the good thing about silicone, I believe few years ago,
there is a dissociation of silicone (reverse polymerization) under some
specific solvent/RH related condition (oil based, If I remember
correctly).  As long as someone fully understand the application, you
will select a good coating for environmental protection.  Otherwise,
there is no "one coating fits all" stuff... May be some grad student
should start a PhD thesis on that...

jk

>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
>Sent: Monday, September 08, 2003 10:31 AM
>To: [log in to unmask]
>Subject: Re: [TN] Silicone conformal coating
>
>
>Of course silicone will repel liquid water, but we are talking
>here of water in a gaseous phase and my experience is that it
>passes small molecules, such as water, like a sieve. In the
>former case, it is a question of the high surface tension of
>water, but single molecules, ata a time, have no surface,
>therefore no surface tension.
>
>Brian
>
>Misner, Bruce wrote:
>> Brian,
>>
>> This diaphram experiment does not take into account the surface
>> wettability of Silicone which is supposed to be one of its major
>> protective features (according to Dow) which precludes surface
>> droplets from forming. Comments?
>>
>> Thanks,
>> Bruce Misner
>>
>>     -----Original Message-----
>>     From: Steve Gregory [mailto:[log in to unmask]]
>>     Sent: Monday, September 08, 2003 8:54 AM
>>     To: [log in to unmask]
>>     Subject: Re: [TN] Silicone conformal coating
>>
>>     In a message dated 09/05/2003 2:03:30 AM Central Daylight Time,
>>     [log in to unmask] writes:
>>
>>
>>>     I thought I had reported the details of this in
>>>     my book, but could not find them today. Must have been
>somewhere
>>> else.
>>
>>
>>
>>     Hi Brian!
>>
>>     It is in your book, on page 329, at the bottom of the
>section where
>>     you talk about Silicone Elastomers.
>>
>>     In your book you state that you made a diaphram of
>silicone that was
>>     5mm thick, and 100mm in diameter. On one side the air
>was held at 40
>>     degrees C., and 95% RH, the other side at 5% RH. There was 1g of
>>     water vapor per day allowed to pass through the silicone
>diaphram.
>>     You stated that is 40 times worse than epoxies, and 20
>times worse
>>     than polyurethanes.
>>
>>     Do you have any idea about arcylics?
>>
>>     Regards,
>>
>>     -Steve Gregory-
>>     ---------------------------------------------------
>>     Technet Mail List provided as a free service by IPC
>using LISTSERV 1.8e
>>     To unsubscribe, send a message to [log in to unmask] with following
>>     text in the BODY (NOT the subject field): SIGNOFF Technet
>>     To temporarily halt or (re-start) delivery of Technet
>send e-mail to
>>     [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>     To receive ONE mailing per day of all the posts: send e-mail to
>>     [log in to unmask]: SET Technet Digest
>>     Search the archives of previous posts at:
>>     http://listserv.ipc.org/archives
>>     Please visit IPC web site
>>     http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>     information, or contact Keach Sasamori at [log in to unmask] or
>>     847-509-9700 ext.5315
>>     -----------------------------------------------------
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a free service by IPC using LISTSERV
>> 1.8e To unsubscribe, send a message to [log in to unmask] with
>following
>> text in the BODY (NOT the subject field): SIGNOFF Technet To
>> temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>> information, or contact Keach Sasamori at [log in to unmask] or
>> 847-509-9700 ext.5315
>> -----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV
>1.8e To unsubscribe, send a message to [log in to unmask] with
>following text in the BODY (NOT the subject field): SIGNOFF
>Technet To temporarily halt or (re-start) delivery of Technet
>send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail
>to [log in to unmask]: SET Technet Digest Search the archives of
>previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>additional information, or contact Keach Sasamori at
>[log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2