TECHNET Archives

May 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 29 May 2012 17:47:56 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Message-ID:
Subject:
From:
Bev Christian <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (116 lines)
Victor,
It is IPC-TM-650 and there is no rev #, as the individual test methods change, not the whole document.
Bev

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Tuesday, May 29, 2012 10:49 AM
To: [log in to unmask]
Subject: Re: [TN] Spot test for Rosin Residue

Was there a Type O in the IPC-TM-65 stated reference #.   Is it TM65 or TM650?  What is the latest Rev.?

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Tuesday, May 29, 2012 9:26 AM
To: [log in to unmask]
Subject: Re: [TN] Spot test for Rosin Residue

Many thanks Brian!!

Rich Kraszewski
PLEXUS 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Thursday, May 24, 2012 1:35 AM
To: [log in to unmask]
Subject: Re: [TN] Spot test for Rosin Residue


  Later: I was fairly sure I had it so did a deeper search and found it 
in chapter 24.2 on p.279, pretty much as I described. I also bring to 
your attention chap. 24.3 on the same page, the IPC acetonitrile test 
which can also be used to detect the presence of rosin. The ref in the 
book was
IPC-TM-65. Test Methods 2.3.38 and 2.3.39, Surface Organic Contaminant 
Detection and Identification Tests, The Institute for Interconnecting 
and Packaging Electronic Circuits, Evanston, II (1984).
obviously updated since then!

Brian


On 24/05/2012 03:18, Bev Christian wrote:
> Rich,
> Check this out.
> http://cool.conservation-us.org/coolaic/sg/bpg/pcc/10_spot-tests.pdf
>
>
> Section 10, Page 24 Spot Tests.  The reference at this point is Barrow 1969,
> 13, TAPPI T408. I did not follow this up.
>
> I have never used the test myself.
>
> Bev
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
> Sent: Wednesday, May 23, 2012 6:28 PM
> To: [log in to unmask]
> Subject: [TN] Spot test for Rosin Residue
>
> I seem to recall a wet chemical spot test for rosin residues.
>
> Something that required:
>
> 	* Piece of filter paper.
> 	* Sugar solution .
> 	* Dilute Sulfuric acid.
>
> If the final spot went red, it would indicate the presence of rosin.
>
> Does anybody recall this test and have the details?
>
> Thanks in advance
>
> Rich� Kraszewski
> Plexus Engineering Solutions
> �
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2