Hi Franklin,
We've actually found more than one way to eliminate mask attack without changing hardener. Variations on a theme, really. Changing hardener seems to have worked for you with your mask system but may not work with some types. I'd recommend changing hardener as the cheapest, easiest way to prevent it, so long as a more resilient hardener is available. Our method works well and adds only a penny to the cost of immersion tin. Process time is not significantly altered and labor is minimal.
Out of curiosity, are you performing tape tests prior to and after bake cycles? We found the propensity for peel the greatest after processing through the immersion line but prior to baking. Using our new method we now get no peel either before or after bake. We're going to test it on immersion Ni/Au soon, as mask peel is also associated with that process as well.
I'd love to share our method with you but we're still modifying it. I'll write you off-line when we've completed all testing if you send me your e-mail address.
Mark
----- Original Message -----
From: Franklin
To: [log in to unmask]
Sent: Friday, July 23, 1999 3:32 PM
Subject: Re: [TN] White Tin land patterns
Mark,
Sounds like you have somlutions we might not have tried. We switched hardners and have not experienced any peeling or brittleness problems. Care to share what you did to solve this, besides the hardener that is.
I'm always trying to find the best method. Thanks.
Franklin
-----Original Message-----
From: Mark Mazzoli <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Friday, July 23, 1999 10:28 AM
Subject: Re: [TN] White Tin land patterns
I see that Franklin has already answered your question about the white tin chemical reaction and application method. I agree with his caution regarding mask and/or legend peel, having experienced the same thing. There are ways of fixing the peeling problem without having to change hardener, however. Any PCB shop setting up an immersion tin process needs to perform adequate tape tests and implement controls before adding this process to their Final Finish list.
As to your other questions, PCB makers differ in their handling of etch compensations. Some like the designer to add the etch factors up front, but most would probably rather do it themselves. Because each of us have slightly different processes, material and equipment we may have slightly different needs insofar as etch factors are concerned. One shop may like to see 1 mil added (for 1 ounce copper surfaces) and another shop may like slightly more or less. It's all a matter of knowing your own process characteristics.
I would venture to say that most shops would prefer that etch factors are not added up front. Most of us would rather do this ourselves.
Hope this helps a little.
Mark Mazzoli
Engineering Manager
Circuit Technologies
[log in to unmask]
3622 Clearview Pkwy.
Atlanta, GA 30340
770-458-1700
----- Original Message -----
From: Ramsey's
To: [log in to unmask]
Sent: Friday, July 23, 1999 5:38 AM
Subject: [TN] White Tin land patterns
With respect to solder protect ant on PWB land patterns, what is "white tin" ?
a.. Is it only tin and alloy or combination of metal and something else?
b.. How is it applied to the land pattern?
With respect to etch back on 1 oz copper. We would like to design boards with lands, for 20 mil pitch QFPs, that measure between 10 and 11 mils wide. Some of our board houses ask us to bump our fab drawings to 12 mil while others asked us not to. Any opinions out there?
|