This one is also available on-line.
On http://www.smtinfo.net/search/search.pl?Match=2&Terms=soldering+to+gold
you'll find this article, plus a few others.
Daan Terstegge
http://www.smtinfo.net
----- Original Message -----
From: "Howard Watson" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, May 13, 2003 11:01 PM
Subject: Re: [TN] ENIG reflow profile vs HASL
> Chris,
>
> There is a really good article in the April 1998 Circuits Assembly:
Soldering to Gold: A Practical Guide, by Ronald A. Bulwith that describes
the considerations when soldering to
> gold finishes, and if you're a magazine packrat like me, you may have this
> issue laying around! It emphasizes what the other members have already
> said, plus it addresses some other issues related to this subject.
>
> Howard Watson
> SMT Manufacturing Engineer
> AMETEK/Dixson
>
>
>
>
> Chris Murphy <[log in to unmask]>
> Sent by: TechNet <[log in to unmask]>
> 05/12/03 05:32 PM
> Please respond to "TechNet E-Mail Forum."; Please respond to Chris Murphy
>
>
> To: [log in to unmask]
> cc:
> Subject: [TN] ENIG reflow profile vs HASL
>
>
> Hi Technetters,
>
> looking through the Technet archives on the differences between HASL and
> ENIG
> boards, I notice that higher temeperatures are required for soldering ENIG
> boards.
>
> Presumably this is because the gold layer firstly has to be dissolved, and
> we are
> dealing with a Ni/Sn intermetallic rather than a Cu/Sn intermetallic.
>
> Does anyone have any recommendations on what differences have to be made
> to the
> reflow profile (e.g. different times above 183 deg C or 200 deg C)? Or
> can the same
> profile be used for the same board regardless of whether it is HASL or
> ENIG?
>
> Thanks in advance for any replies.
>
> Regards,
>
> Chris Murphy,
> Production Engineering,
> Tait Electronics
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|