Frank Kriesch <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 27 Apr 2010 09:45:41 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (152 lines)
Hi,

i know "SMT Quattro Peak".

SMT is a German producer of Solderingequipment, e.g. Reflowofens.

Find more on: http://www.smt-wertheim.de/smt.html

Kind regards

Frank Kriesch




Von:
Ioan Tempea <[log in to unmask]>
An:
[log in to unmask]
Datum:
26.04.2010 21:21
Betreff:
Re: [TN] SMTA quattro Peak C3.0
Gesendet von:
TechNet <[log in to unmask]>



Hi Steve,

This is a reflow oven. Somebody has some in stock and I was wondering if 
it could be a good buy or not.

Best regards,

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] 
W | www.digico.cc

N'imprimer que si nécessaire - Print only if you must


-----Message d'origine-----
De : Steve Gregory [mailto:[log in to unmask]] 
Envoyé : April-26-10 2:42 PM
À : 'TechNet E-Mail Forum'; Ioan Tempea
Objet : RE: [TN] SMTA quattro Peak C3.0

Hi Ioan!

Just by me asking this question will tell you that I'm not a user, but 
what
is this?

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Monday, April 26, 2010 9:01 AM
To: [log in to unmask]
Subject: [TN] SMTA quattro Peak C3.0

Dear Technos,

 

Any users of this brand? What is your feedback?

 

Thanks,

 

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] <mailto:[log in to unmask]> 
W | www.digico.cc <http://www.digico.cc/> 

 
 N'imprimer que si nécessaire - Print only if you must

 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------




.
Der Inhalt dieser E-Mail ist für den Absender rechtlich nicht verbindlich.
Informieren Sie uns bitte, wenn Sie diese E-Mail fälschlicherweise erhalten haben (Fax: +49-7551-891-4001). Bitte löschen Sie in diesem Fall die Nachricht. Jede Form der weiteren Benutzung ist untersagt.
.
The content of this e-mail is not legally binding upon the sender.
If this e-mail was transmitted to you by error, then please inform us accordingly (Fax: +49-7551-891-4001). In such case you are requested to erase the message. Any use of such e-mail message is strictly prohibited.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2