TECHNET Archives

December 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Graham Naisbitt <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 1 Dec 2000 16:47:07 -0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (65 lines)
Joe

HumiSeal have EXACTLY what you are looking for.

Contact them via www.humiseal.com

Phone 718 932 0800
Fax  718 932 4345

Hope this helps

Regards
Graham Naisbitt
[log in to unmask]
Web: www.concoat.co.uk
Concoat Ltd
Alasan House, Albany Park
CAMBERLEY GU16 7PH
Tel: +44 (0) 1276 691100
Fax: +44 (0) 1276 691227

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Kane, Joseph
Sent: Friday, December 01, 2000 02:43
To: [log in to unmask]
Subject: [TN] Conformal Coat Masking


Can anyone out there recommend a good masking tape?

Desired properties, in approximate order of importance:
1. Withstands 85C indefinitely.
2. Sticks well, but peels off without leaving residue.
3. Antistatic a plus, but conductive probably not worth it (we
    use ionizing air blowers).
4. Inexpensive.

Our coatings are mostly urethanes, manually sprayed.

Joe Kane
BAE SYSTEMS Controls
Johnson City, NY

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2