TECHNET Archives

December 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Andy Magee <[log in to unmask]>
Reply To:
Date:
Fri, 18 Dec 1998 21:07:26 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (38 lines)
Michael,

Excellent posting. I really appreciate a reasoned approach to an
engineering challenge.

We did quite a bit of work for CERN (Claude-Pierre Marin) a few years
back on coverfilm and adhesive based laminate. The most reliable
adhesive for long term exposure to liquid helium in the ATLAS detector
was phenolic-butyral. (Though it ultimately wasn't selected for other
reasons.) It's stiffness and adhesion properties were very stable at all
cryogenic temperatures.

In a separate study for BEI we discovered that Acrylics were only useful
down to about -35C. At -50C the bond strength was completely
compromised.

Your observations of an "aging" effect may be the result of polymer
oxidation. Also, be careful to investigate the source of the opens. Is
it a lack of support by the coverlay, or simply a failure of the
adhesiveless laminate bond at cryogenic temperatures?

Andy Magee
Flex Guru - Consulting
[log in to unmask]
(937) 435-3629

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2