Chris ,
acrylic is not accepted by the customer, because it does not withstand the harsh environment (alcohol from de-icing wings, nor jet petrol and other stuff)
Inge
From: [log in to unmask]
Sent: den 12 March 2010 11:00
To: Inge
Cc: [log in to unmask]
Subject: Re: [TN] Vibration issue
Is acrylic conformal coat a possibility for you? Has solved some vibration issues for us.
Best Regards,
-Chris
Inge <[log in to unmask]>
Inge <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/12/2010 01:47 PM Please respond to
Inge <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Vibration issue
Hi all,
we are making a very vital part for a aircraft builder. Problem with
TQFPs, some 200 legs. There are resonance peaks that kill the package legs.
Redesign is not to think of from the customer, so we must do something on
inside of the box. One solution (not popular) is to use a string of a glue
along the leg rows in order to lock them. Another is to place a vibration
dampening mat on one side of the board. That one is more tricky , but there
is a US company with lots of stuff for that purpose. Anyone with
experience from this area? I should add that not all legs are broken, just
one or two after 100 hs of random vibration, but that is of course not
acceptable. BGAs would solve the problem, but there is no time for
redesign.
I'm sorry for coming with a serious message at this holy time of the week.
Thanks
/Inge
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
This e-mail message is intended only for the use of the intended recipient(s).
The information contained therein may be confidential or privileged, and its disclosure or reproduction is strictly prohibited.
If you are not the intended recipient, please return it immediately to its sender at the above address and destroy it.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|