TECHNET Archives

July 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Victor Hernandez <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 12 Jul 2011 09:36:21 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (36 lines)
Fellow TechNetters:

   I did not receive many responses to mu original inquiry, so I will post again.   I hope someone will contribute or lead to to some solid information/data/article regarding the process of ceramic thin Film process.   I will post a conceptual photo I what I am searching for with Steve.

Victor,

_____________________________________________
From: Hernandez, Victor G
Sent: Friday, July 01, 2011 9:59 AM
To: TechNet E-Mail Forum
Cc: Hernandez, Victor G
Subject: Thin Film Ceramic Resistor, 51K, serpentine


Fellow TechNetters:

   Do anyone out there have experience/knowledge of the ceramic resistor process and parameter specification?  Is there a base material applied before thin film application?    Is there a method/technique for checking coating integrity.   Similar to, Chemical test for passivation pin hole on ICs.  Is there a spec for end cap/wrap around?  Etc....

Victor,


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2