We used high temp solder for profiling the wave solder ovens (we had the
wave turned off - not sure if the high temp solder would survive it)
We have also been using a Thermal conductive adhesive aluminum tape witch
seems to work well when covered in Kapton.
Samuel Ares
Process Engineering
Leitch Technology Int.
[log in to unmask] <mailto:[log in to unmask]>
(416) 445-9640 x. 3395
-----Original Message-----
From: Kathy Kuhlow [SMTP:[log in to unmask]]
Sent: Tuesday, February 13, 2001 3:02 PM
To: [log in to unmask]
Subject: Re: [TN] Thermal profiles at Wave Solder
I have always attached the wires using Kapton tape or clips.
Kathy
>>> [log in to unmask] 02/13/01 12:36PM >>>
Good Afternoon,
When profiling assemblies at wave solder what is the preferred
method for
attachment of thermocouples?
Glue
Kapton tape
Thermal conductive adhesives
High temp solder
Destructive - Thermocouple embedded in PCB
Just curious on some of the answers I may receive........
Thanks in Advance
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
----- << File: TEXT.htm >>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|