Sender: |
|
X-To: |
|
Date: |
Thu, 27 Jan 2000 05:00:00 EST |
Reply-To: |
|
Content-type: |
text/plain; charset=US-ASCII |
Subject: |
|
From: |
|
Content-transfer-encoding: |
7BIT |
In-Reply-To: |
|
Organization: |
CALCE EPRC |
MIME-Version: |
1.0 |
Parts/Attachments: |
|
|
Ralph,
A good bet is to talk to the people at Thermagon. They produce
laminate material with a thermal conductivity of 3 to 5 W/m-C, more
than 10 times the conductivity of normal FR-4.
Craig
Date sent: Mon, 24 Jan 2000 15:26:13 -0600
Send reply to: [log in to unmask]
From: Ralph Garvin <[log in to unmask]>
Organization: Westport Research Associates, Inc.
Subject: Re: [TN] PCB SUBSTRATE MATERIAL;
To: [log in to unmask]
> attn: ALL
>
> I have a question regarding pcb laminate materials. We are looking
> for a material with a high thermal conductivity.
>
> If there is anyone out there with knowledge of such or links to same,
> it would be appreciated.
>
> Thanks in advance.
>
> Ralph Garvin
> New Product Development
> Westport Research, Inc.
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c ############################################################## To
> subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body: To subscribe: SUBSCRIBE TECHNET <your
> full name> To unsubscribe: SIGNOFF TECHNET
> ############################################################## Please
> visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information. If you need assistance - contact Gayatri Sardeshpande at
> [log in to unmask] or 847-509-9700 ext.5365
> ##############################################################
Dr. Craig Hillman
CALCE Electronic Products and Systems Consortium
University of Maryland
College Park, MD 20742
(301)-405-5316
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|