Hello
The boards are HASL  class 2 that are used in the telecommunications
industry. We had a solder guru in and he stated that the boards did not
appear to be cleaned properly. He talked about organic flux wash,then  hot
water wash at a specified temp of at least 140 degrees and finally a blow
dry.  The boards are single sided that we put air coils and caps into.
Thx's Tom
-----Original Message-----
From: [log in to unmask] <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>; [log in to unmask]
<[log in to unmask]>
Date: Wednesday, September 22, 1999 10:49 AM
Subject: Re: [TN] Fw: Cleaning of Boards at Board Manufacturer


>Tom:
>
>Many of these cleaning issues will vary with the sort of surface finish on
>the pads.
>
>Typically, Electroless Nickle Gold will get only a water rinse, whereas Hot
>Air Leveled boards often get a thorough alkali cleaning.
>
>So to get good answers, you must specify what your surface finish is.
>
>Rudy Sedlak
>RD Chemical Company

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2