TECHNET Archives

October 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"(No Name Available)" <[log in to unmask]>
Date:
Thu, 22 Oct 1998 16:00:16 EDT
Content-transfer-encoding:
7bit
Content-type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (28 lines)
Hi Technetters,
It is time to ask advice from the experts so here I am.  I need some help, as
usual.  I think I need you guys and gals about once a month.  Thanks for being
here.

Here is the problem.  If you have a board that has 15 mil pitch should the
board be tin/lead plated or should it have a flash of gold?  I have heard that
gold flashing is a must for 15 mil boards.  So tell me, what is the answer.
Also if you had any problems and solutions you would like to share with this
pitch of component.

Thanks in advance,

Linda Zellars
[log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2