TECHNET Archives

February 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Sauer, Steven T." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 21 Feb 2002 15:23:23 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (33 lines)
Phil,
The simplest method is to dip the wire in a solder pot (~500°F, 260°C).
This removes the coating and tins the wire at the same time.  Most 
polyurethanes and nylon coatings are in thermal classes of 105°C, 130°C,
155°C and 180°C which should be removable while immersed in molten solder.
The dwell time will be significantly longer than what is used to tin
temperature sensitive components.
Another method is thermal strippers.
The least favorite and hardest to control is abrasion using an exacto knife.

Steve Sauer
Manufacturing Engineer
Northrop Grumman, Xetron

-----Original Message-----

Anyone have a reliable safe method of removing the polyurethane and nylon
coating that protects magnet wire so that the wire can be used to solder as
a jumper wire.  I remember using a hot chemical salt type stripping bath
many years ago but was hoping that someone has found a better way to do
this since then.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2