TECHNET Archives

July 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Tempea, Ioan" <[log in to unmask]>
Date:
Thu, 10 Jul 2003 08:29:12 -0400
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Parts/Attachments:
text/plain (33 lines)
Hi technos,

I have run into trouble with a PSS connector from Samtec. Before reflow it
is OK, can't see any cracks in all the parts I checked in the tubes, but I
get major cracking of the pins, randomly, after reflow. Please see the
picture at http://www.stevezeva.homestead.com/files/crackedpin.jpg, another
friendly support from Steve G.

What could cause that? It is an established product, we already built
thousands with no trouble. Could it be the reflow recipe causing this? Maybe
it was borderline and for some reason it is too hot now. It is not the
joint, but the actual pin that cracks. Actually, can the thermal excursion
give this?

Or is it some tension built in the pins from bending at the connector
manufacturing level, maybe the material was tempered somehow?

Any clue would be appreciated.

Thanks,
Ioan

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2