TECHNET Archives

February 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Douglas O. Pauls" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 11 Feb 2004 07:33:04 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (179 lines)
Good morning Daan,

Where did you ever get that idea?  Must have been one of those mornings
before I had my Diet Dew(s).

Residues on components or bare boards is always an issue.  If the residue
on either is a purely surface residue, then it is less of a concern if they
are going into a no-clean assembly operation.  It is more of a concern, or
critical, in no-clean assembly because you have no way of addressing those
residues.

If the components or boards have absorbed residues, you are toast.  You
"might" be able to do rescue cleaning in mild cases, but most often not.
The laws of physics are not subject to repeal or negotiation.

Doug Pauls



                                                                                                                                              
                      "d. terstegge"                                                                                                          
                      <[log in to unmask]        To:       [log in to unmask]                                                               
                      SGROUP.COM>                     cc:                                                                                     
                      Sent by: TechNet                Subject:  Re: [TN] Contamination on a SOT-23 component                                  
                      <[log in to unmask]>                                                                                                       
                                                                                                                                              
                                                                                                                                              
                      02/11/2004 03:16 AM                                                                                                     
                      Please respond to                                                                                                       
                      "TechNet E-Mail Forum.";                                                                                                
                      Please respond to "d.                                                                                                   
                      terstegge"                                                                                                              
                                                                                                                                              
                                                                                                                                              




Hi Brian,

I understood from earlier posting of you and others that the lack of
cleanliness of incoming components is considered a risk ONLY for
no-clean technology.  Now Cheryl obviously has a problem with
contaminated parts in a process that does include cleaning. This makes
me wonder how (in general) the chances are that a cleaning process
designed mainly for cleaning flux residues from pcb assemblies will
clean the variety of contaminants present on incoming parts. Perhaps you
can comment on this ?

Daan Terstegge
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net

>>> [log in to unmask] 02/11/04 08:56am >>>
Amen! Lord Doug has hit it on the head.

It may interest you (academically) to know that the erstwhile company
I
owned manufactured the Microcontaminometer 20 years ago, through to
1991. It was capable of measuring the ionic contamination on parts as
small as a single diode. It was not a popular instrument: I think we
probably sold less than 50 of the beasts. What we did find was that
many
components were hopelessly badly contaminated. There is a whole
chapter
in my book on this subject, with photos. One IC, which is shown,
measured at 12.4 µg/cm2 eq. NaCl and this is by no means exceptional.

My experience in my former professional life was that component
manufacturers cared even less about cleanliness than they did about
solderability and I know no reason why this state of affairs should be
any different today.

Brian

Cheryl Tulkoff wrote:

> I've been working on a tough but challenging contamination problem.
The
> contamination causes electrical leakage fails on a precision test
> instrument. Ion chromatography analysis points to an incoming
cleanliness
> problem on a SOT-23 component. Elevated choride and sulfate levels
were
> found on the components (5x - 10x greater ug/in2 levels than
anything
> found elsewhere on the boards). High levels were found even on our
"good"
> boards.
>
> We are trying to work with our supplier to identify and fix the
problem
> long term but are looking for some short term fixes as well.
Repeated
> water washing of the boards (high pressure spray cleaning) improves
the
> situation but does not fix it. Alcohol scrubs in the area further
improve
> it but don't eliminate the problem entirely.
>
> We have a only a DI water wash process (no surfactant/saponifier
> capability).Does anyone have any board or component cleaning
> recommendations?
>
> Are there any parts makers out there willing to tell me a little
more
> about parts cleaning after the lead plating process?
>
> What tool(s) do part makers use to verify cleanliness of parts?
>
> I don't have a tool capable of measuring what was found on the part
so I
> don't know where to go.
>
> Thanks, Cheryl Tulkoff
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following
text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (M
AIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2