Rick,
I'd have to disagree with Jim. We have many customers that have used
Durapol through reflow with no issues. The esd versions of Delmat,
Durastone, and Durapol are all temperature specified at or around 300
degrees Celsius and are non-flammable. I do agree Jim on a full process
fixture as opposed to reflow only to address some of your concerns.
Chad
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of jim
Sent: Wednesday, May 07, 2003 11:05 AM
To: [log in to unmask]
Subject: Re: [TN] Reflow Fixture Opinions Sought
Rick,
You cannot use Durapol in the reflow oven. It will burn up in just a
hundred
or so passes. You need to use Durastone or Delmat.
You may also want to consider using a fixture that you can run through
the
screen printer to avoid handling after printing.
Jim
----- Original Message -----
From: "Rick Thompson" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, May 07, 2003 12:48 PM
Subject: [TN] Reflow Fixture Opinions Sought
We have a customer who is requesting that we use a reflow fixture
consisting
of a Durapol plate with removable tooling pins to accomodate several
different large PWBs through the reflow process. These fixtures would
run on
the flat belt rather than edge rails and would require that we remove
large
(16"x12") fully loaded boards from the conveyor rails to install on
these
fixtures prior to reflow. Components on the board range include a number
of
BGAs and micro-BGAs. The intent of the fixtures is to keep the board
from
flexing during reflow. My concern is that all the handling and flexing
of
boards with components in solder paste is going to increase the chances
of
soldering problems due to part separation from the paste if the board is
flexed.
Question: Has anyone used this type of concept on large, densely
populated
boards. Comments on pros and cons? Any other insights would be
appreciated
as I'm looking for supporting evidence to dissuade them from this
approach
which is primarily aimed as saving fixture costs over dedicated SMT
fixtures.
Thanks in advance.
Rick Thompson
Sr. SMT Process Engineer
SMTEK International, Inc.
+1 (805) 532-2800
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|