Hi Frank - No, I wouldn't recommend replacing the nickel with copper.
Copper will diffuse into/through the Ag finish creating an unsolderable
condition after an extended amount of time. The "extended" amount of time
will depend on the storage/use/handling conditions for the parts. You can
find some good info in Klein Wassink's book "Soldering in Electronics" ISBN
0-901150-14-2 on this issue. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]





GuitarBud <[log in to unmask]> on 05/02/98 12:42:37 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to GuitarBud <[log in to unmask]>

To:   [log in to unmask]
cc:    (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
Subject:  Re: [TN] Ni plating and Immersion Au




I am plating stamped 1018-Steel parts with Ni and then Ag.  I am then
soldering them together with 2%Ag solder.  It is roughly 1" x 8".  Should I
use Cu in place of the Ni?

Frank

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2