Although you inhabit a different world than I do (you are in the real world,
I am in a theoretical cubicle), I still have to question this philosophy. If
an electrical engineer has determined that he needs a 50mil gap (after
derating for fab allowances, of course), and some kind of plating or
contamination problem has reduced the desired 50 mil gap to a slightly over
the 6-10mil minimum you used in your example, and your inspectors are
trained to only look at the minimum, then acceptance of these boards could
be a risk, in my mind.
I'm not suggesting that your inspectors need to know the intent of the
designer, but this example is clearly rejectable in IPC-A-600 2.10.1.2
I'm just sayin'....
Jack
.
On Thu, Feb 17, 2011 at 10:08 AM, Stadem, Richard D.
<[log in to unmask]>wrote:
> Standard industry practice is to put the minimum electrical clearance for a
> given CCA on the fabrication drawing of the PWB for that CCA. It typically
> ranges from .006" to .010". Of course, it depends (TM) on the design,
> application, and use environment. The assembly operators and inspectors for
> my client companies are trained to inspect to that minimum clearance, reject
> if violated, and then the ME/QE|DE|Customer FAI disposition as to whether it
> is to be reworked or use-as-is.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
> Sent: Thursday, February 17, 2011 9:51 AM
> To: [log in to unmask]
> Subject: Re: [TN] Electrical Clearance as stated in IPC standards
>
> I agree with what Gary says in principle. Clearances set by voltage
> requirements will be much larger than MINIMUM clearances for different
> classes
> in IPC.
> But I have to comment that since the scenario put forth by Wee Mei stated
> "during bare board inspection (class 3 requirement)", if the defects are
> rejectable by criteria in IPC-A-600, then the boards are rejectable.
> period.
> What I mean is, an inspector can't be expected to know what the circuit is
> intended to do, and if manufacturing defects violate the criteria, its
> rejectable.
> If someone else wants to evaluate the situation and determines that the
> defect won't affect the circuit performance, then the boards MAY be
> accepted
> anyway.
> Your quote said "the argument kick-in that it is not a violation and can be
> acceptable" is half right. It CAN be acceptable, but it IS a violation.
> I hope the manufacturer is not bullying you into accepting defective boards
> based on knowledge of the circuit, telling you not to worry about the
> defect
> because the circuit should still work okay. It should be the customer that
> makes that decision, right?
>
> Jack
>
> .
>
> On Thu, 17 Feb 2011 10:14:10 -0500, Gary Ferrari
> <[log in to unmask]> wrote:
>
> >Lum Wee Mei,
> >
> >Minimum electrical clearance is based on the voltage used in the design.
> >The greater the voltage, the greater the required spacing. In your
> >example, the spacing used was much larger than the required minimum
> >electrical clearance, based on voltage. Although the defect reduced the
> >spacing beyond what is considered acceptable, per the artwork, the end
> >result still did not violate the voltage based electrical clearance. In
> >this case, the board may be accepted, this time. The supplier should not
> >count on you accepting such product quality in the future.
> >
> >Regards,
> >
> >Gary F.
> >
> >On 2/17/2011 12:26 AM, Lum Wee Mei wrote:
> >> Dear All,
> >>
> >> Until now, I am still very curious about this term "electrical
> clearance" that
> is used on the IPC standards. Very often, the standard will says something
> like
> "it is acceptable as long as it meets the electrical clearance". As I did
> not have
> the IPC standards with me when I right this, allow me to use a scenario to
> illustrate my query :
> >>
> >> A digital PCB has some pockets of power and ground area fills with
> minimum
> trace width/clearance of say 6mil/6mil (0.15mm/0.15mm) and power trace
> width of 50mil. During bare board inspection (Class 3 requirement), one of
> the
> power trace that run along side of the ground fill, has an excessive copper
> protrusion that reduce the physical conductor to conductor clearance by
> 60%.
> Based on the IPC-A-600, it has violate the conductor to conductor
> clearance.
> However, the argument kick-in that it is not a violation and can be
> acceptable
> because the remaining clearance of 40% is much larger than the electrical
> clearance stated in IPC-2221 for that application. Now, how should this be
> resolved?
> >>
> >> Thanks and Regards,
> >> ~ Wee Mei ~
> >>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|