TECHNET Archives

January 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=US-ASCII
Sender:
Subject:
From:
Cheryl Tulkoff <[log in to unmask]>
Date:
Thu, 15 Jan 2004 09:40:27 -0600
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Morse, Carrie" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (132 lines)
Joe  -

As a long time and now former user of this flux, this is not the only issue
that you may face while using it. It is an extremely aggressive OA flux - I
never came across a stronger OA flux on the market (acid number of 60, 3%
chlorine, pH of 3).  It works great even on difficult to solder boards -
old stuff, Cu with OSP finishes, etc. However, it will erode most grades of
stainless steel and will flat out eat up any aluminum. Titanium was the
metal of choice for any fixturing that came in frequent contact with this
flux.

So, look out for eroding metal on your conveyor rails and preheaters. Also,
if you use spray fluxers, you will need to keep an eye on any metal
surfaces and upgrade them or change to nylon or something similar.


Cheryl Tulkoff
Phone:(512) 683-8586
Fax: (512) 683-8847
National Instruments
11500 N. Mopac Expressway
Building A
Austin, TX 78759-3504





                      "Morse, Carrie"
                      <CMorse@CIRTRONIC        To:       [log in to unmask]
                      S.COM>                   cc:
                      Sent by: TechNet         Subject:  Re: [TN] Solder Sticking To SS Screws
                      <[log in to unmask]>


                      01/15/2004 09:26
                      AM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to
                      "Morse, Carrie"






Joe,
We use OA flux and do not have a problem with SS screws.  Anyone else out
there having a problem with OA flux and SS hardware? (Make sure they are SS
and not Zinc Plated or something else.)

Latex mask is easy to use and we have found a mask that is not messy.
We apply it straight from the bottle or using a dispenser.

Kapton dots can also be used -- those are a bit neater, but, a bit more
expensive.

Nylon screws do exist and we do not have problem with those going thru wave
either.

-Carrie

-----Original Message-----
From: Kane, Joseph E [mailto:[log in to unmask]]
Sent: Thursday, January 15, 2004 10:20 AM
To: [log in to unmask]
Subject: [TN] Solder Sticking To SS Screws


Because connector screws get Loctite, we use stainless steel temporary
hardware on bottom sides of some of our motherboards, and screw heads and
washers travel through the solder wave.  With the switch from RMA to OA
flux (Alpha 3355-HB), we find that solder now adheres to the hardware.
Here are some of our options:

1. Use latex temporary solder mask on hardware.  Of course, this will be
messy and labor-intensive.

2. Find some 2-56 x 1/2" screws in a material that Sn63 won't stick to.
Could they make a screw this small in nylon or diallyl pthalate?

3. Apply some kind of plating or Teflon coat.  Of coarse, with buildup on
the thread, they may not mate anymore.

4. What about a spray-on coating?  Would it be worth trying an anti-seize
like  molybdenum disulfide?

Joe Kane
BAE SYSTEMS Controls
Johnson City, NY


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest