Tucker, Steve (KS) wrote:
>
> Hello Technetters,
>
> I have been experiencing considerable defects across the wave solder with
> one particular vendors PCB's. My question is what guidelines are most
> commonly used to perform a solderability analysis and can anyone suggest a
> good lab for having this done.
>
> Thanks in advance,
>
> Steve Tucker
>
> Name: WINMAIL.DAT
> Part 1.2 Type: unspecified type (application/octet-stream)
> Encoding: x-uuencode
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ##############################################################
Steve,
I suggest you review IPC-6012, Para 3.3.6 Solderability and J-STD-003
This paragraph describes testing for solderability of PWB's and
conditions to test for solderability for length of time PWB's must be
solderability prior to assembly. Knowing the type of business you're
involved in condition "C" might be a good choice. Be sure you add a
note to your procurement drawings calling out this requirement. At
least require a wave soldering test prior to delivery and after receival
as an acceptance requirement. Again add this requirement to the
procurement drawing.
Regards,
Arny Andrade
Sandia Labs, Ret
e-mail [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|