Jim,
appreciate if you can fax one copy to me too, my fax number is : (65)
2903184...Thanks.
Regards,
Fung Leng
Micron Semiconductor
------------------
Original text
From: "Vaughan, Ralph H" <[log in to unmask]>, on 21/10/1998 8:53
AM:
Jim,
You should know better than to offer anything free to this Technet crowd. I
would also appreciate a fax of your chart. thanks.
Ralph Vaughan
Boeing
Fax 770 497-5555
> ----------
> From: James R. Paulus[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;[log in to unmask]
> Sent: Wednesday, October 21, 1998 11:13 AM
> To: [log in to unmask]
> Subject: Re: [TN] FR4 thermal expansion
>
> I have a comprehensive chart which I can fax you, if you want to provide
> the
> phone #.
> Generally, Z-axis is 60 to 80 ppm (or microinches/inch/C), X is 17-20 ppm,
> and
> Y is 15 to 18 ppm. Lots of variables however:
> a. These values are for a temp ramp up to the Tg, which is 135C typically
> for
> FR4.
> b. Remember that FR4 today can be a material with a Tg as high as 180C.
> Higher Tg FR4's tend to exhibit a slightly lower Z-expansion below the Tg
> than
> 135C types.
> c. Z-axis is particularly affected by resin:glass ratio. Higher Resin
> content means greater expansion, which has to be considered in high layer
> count designs.
> d. Above the Tg, the X and Y movements get squirrelly because the
> softened
> resin allows the glass fabric to pull back against the expanding matrix,
> resulting in much lower values.
> jimpaulus
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|