TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Date:
Thu, 27 May 2010 14:16:39 +0000
Reply-To:
Subject:
From:
vladimir Igoshev <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Type:
text/plain; charset="Windows-1252"
Content-Transfer-Encoding:
base64
Parts/Attachments:
text/plain (1 lines)
Ioan,
You'd have to go through the whole process of testing to confirm your process is "clean". We can do it for you as we have an XRF machine (Fischer XDAL) for the tests.

Regards,
Vladimir

SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca

-----Original Message-----
From: Ioan Tempea <[log in to unmask]>
Date:         Thu, 27 May 2010 09:38:36 
To: <[log in to unmask]>
Subject: [TN] Cross contamination of RoHS boards

Dear Technos,

 

Did anyone perform contamination testing of RoHS boards? I mean, we would like to have hard evidence telling where to draw the line: can we re-use SnPb stencils for RoHS, can we use the same cutters, picks , crimpers, lead forming dies, press-fit tooling, wave pallets, etc? I know the "better safe than sorry" policy is the best, but at times scrapping all the tooling sets for a product becomes very expensive!

 

Are there any reports, even pay ones, dealing with this topic?

 

Thanks,

 

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] <mailto:[log in to unmask]>  
W | www.digico.cc <http://www.digico.cc/> 

 
 N'imprimer que si nécessaire - Print only if you must

 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2