TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Howieson, Rick" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 9 Feb 2000 10:37:33 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (60 lines)
Steve,
Is there a serial number on the board that may identify it to a
particular panel. If so, and you may need to contact the fabricator,
find if you have boards from the same panel and check those, closely,
for any delamination.
Rick
GTC

>-----Original Message-----
>From:  Stephen R. Gregory [SMTP:[log in to unmask]]
>Sent:  Wednesday, February 09, 2000 10:13 AM
>To:    [log in to unmask]
>Subject:       [TN] Delamination
>
>Hi ya'll!
>
>We just finished building a lot of 48-boards through SMT. Out of that 48
>there was one board that we just discovered a big delamination blister on the
>backside...it's about 1.5" wide and maybe 2.5 - 3" long. There was no rework
>done on the board, and it was reflowed under the same profile in a
>Conceptronic HVA-70 that the rest of them were...and they don't exhibit any
>problems. There no sign of overheating at all around the blister, and the
>silkscreen is nice and bright white...we just have this big blister. What
>might cause that? The boards are polyimide. We didn't bake them, and they
>were real fresh boards date code was 0300. Like I said, it was the only board
>that had a problem...the rest are fine.
>
>TIA
>
>-Steve Gregory-
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2