TECHNET Archives

July 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"FOX, Ian (York Rd)" <[log in to unmask]>
Date:
Mon, 14 Jul 2003 08:46:22 +0100
MIME-Version:
1.0
X-To:
Kaye Clayo <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "FOX, Ian (York Rd)" <[log in to unmask]>
Parts/Attachments:
text/plain (73 lines)
Kaye, the addition of material to the exterior surfaces of PCB's does little
to prevent moisture absorption. If you carry out periodic weight gain
measurements under RTCA DO160 humidity testing conditions (we always use
category B, the 10 day test) on a resist coated PCB,  you find that better
coating materials reduce the absorption rate by about 20%, most by 10%, but
after 4 days of humidity exposure the PCB's are just about saturated (that
equates to about 0.7% for a basic FR4 and 2% plus for some aramids),
irrespective of what you have on the outside. Hope this is of some help.

Regards
Ian Fox
Goodrich Engine Controls

-----Original Message-----
From: Kaye Clayo [mailto:[log in to unmask]]
Sent: 11 July 2003 16:38
To: [log in to unmask]
Subject: [TN] Low moisture absorbing soldermask


Dear Technet:

I have just been asked if there is a soldermask that has a low moisture
absorption property. We have a pcboard that uses Taconics TLC material,
which is absorbing moisture, and the engineer would like to "encase" the
board with a low moisture absorbing soldermask to solve this problem.

Does anyone know of anything that will work, or another way around this
problem?

The engineer also asked me if anyone knew how to relate IPC-TM-650 2.6.2.1
"Water Absorption, Metal Clad Plastic Laminates" to real life. What he means
is, how does this test method, which dunks a pcboard into distilled water
for 24 hours, relate to 70% humidity at 23C.

Thank you for your help.

Kaye Clayo
Sr. P. C. Board Designer
Keithley Instruments, Inc.


CONFIDENTIALITY NOTE: This message is intended only for the use of the
individual or entity to which it is addressed and may contain information
that is privileged, confidential, and exempt from disclosure under
applicable law. If the reader of this notice is not the intended recipient,
you are hereby notified that any dissemination, distribution or copying of
this communication is strictly prohibited. If you have received this
communication in error, please notify the sender immediately.

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/html/forum.htm for additional information, or
contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2