TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Rex Waygood <[log in to unmask]>
Date:
Tue, 25 May 2010 15:04:38 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Eric CHRISTISON <[log in to unmask]>
Content-Transfer-Encoding:
8bit
Subject:
From:
Eric CHRISTISON <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (314 lines)
Don't think so Rex.

Certainly it's the way my company operates and our biggest customer 
operates the same way. We get the ROHS breakdowns from our suppliers, we 
put them all together into a big spreadsheet and send them to our 
customer who collects all the ROHS spreadsheets from all the other 
suppliers they use and put them all together into an even bigger 
spreadsheet.

To my almost certain knowledge my (multinational) employer has never, 
ever, carried out a chemical analysis on a supplier's material for the 
purposes of establishing ROHS compliance and we sell our products 
worldwide, including the litiginous USof A.

You wouldn't expect a mobile phone supplier to carry out it's own 
chemical analysis of every single component it puts in a phone.

Regards,



On 25/05/2010 14:40, Rex Waygood wrote:
> But it would be RIM that ended up in court or with a recall situation if non compliant.
>
> I do not believe a defence of Due Diligence is acceptable in all EU countries. It is under UK law.
>
> Only RIM can decide upon what precautions (Due Diligence) are suitable for their costs, risks, markets and products.
> In UK law RIM would use that as part of their defence. In other countries it would make no difference, the offense has been committed.
>
> Regards
> Rex
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Eric CHRISTISON
> Sent: 25 May 2010 14:31
> To: [log in to unmask]
> Subject: Re: [TN] RoHS compliance of stainless stell
>
> You should be able to get an ROHS chemical breakdown from the supplier, ultimately in your case it would be the steel mill who will do a chemical analysis of what they make anyway.
>
> RIM shouldn't have to go out and get an analysis done themselves, get your vendor to do it. It's what you pay them for. Of course that should be clearly explained in the procurement spec and the purchase order...
>
> Regards,
>
>
>
> On 25/05/2010 14:13, Rex Waygood wrote:
>    
>> Short answer
>> CoCs from a trusted vendor are considered by many as adequate for our industry.
>>
>> Due Diligence is different depending upon who you are, what the risks are, and the difficulty of doing the test.
>> Due Diligence is also not defined legally anywhere (I have a vague feeling that it only has any use inside the UK).
>> You must decide and be able to defend your choice of Due Diligence.
>>
>> Rex
>>
>>
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
>> Sent: 25 May 2010 13:25
>> To: [log in to unmask]
>> Subject: Re: [TN] RoHS compliance of stainless stell
>>
>> Rex,
>> CoCs only are not enough to satisfy the EU's definition of "due diligence" (I hate that term).  When I asked what more I need to do, the answer I received (from the UK Department of Trade&   Industry - now changed to BER, whatever that stands for) was "the courts will decide". Yeah, sure, like I want to go to court to find out!
>>
>> So, working for a company with some deep pockets, we do a LOT of testing. I have no clue how they expect little companies to do more than collect CoCs.
>> Bev
>> RIM
>>
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Rex Waygood
>> Sent: Tuesday, May 25, 2010 8:20 AM
>> To: [log in to unmask]
>> Subject: Re: [TN] RoHS compliance of stainless stell
>>
>> Approved vendor/Trusted source + CoC
>>
>> Rex Waygood
>> Technical Manager
>>
>> Hansatech EMS provides value manufacturing through engineering and
>> quality
>>
>> Hansatech EMS Limited
>> Benson Road
>> Nuffield Industrial Estate
>> Poole
>> Dorset
>> BH17 0RY
>>
>> +44 (0)1202 338200
>>
>>
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
>> Sent: 25 May 2010 13:14
>> To: [log in to unmask]
>> Subject: Re: [TN] RoHS compliance of stainless stell
>>
>> Thanks Bev!
>>
>> So after a tough week-end with the Habs being cut off this year's Stanley Cup final I find out one of my front runners, Bacardi, could be lead poisoning. Despicable! But, luckily, I only purchase liquors in glass bottles, so this one is taken care of, or at least I hope the Pb in glass is stable!
>>
>> To summarize to date:
>> SS has no issue with Pb and CrVI
>> Cd as an alloying element for SS has not been mentioned and can't find
>> any related texts on Internet either, so I guess I will consider no Cd
>> in SS Because of austenitic vs martensitic nature of SS, magnets are
>> not exactly the best way to validate RoHS compliance
>>
>> Now, I think you've seen it coming: how do you assess the compliance of the SS parts you're using? CofC only?
>>
>> Thanks,
>>
>> Ioan Tempea, ing.
>> Ingénieur Principal de Fabrication / Senior Manufacturing Engineer T |
>> 450.967.7100 ext.244 E | [log in to unmask] W | www.digico.cc
>>
>> N'imprimer que si nécessaire - Print only if you must
>>
>> -----Message d'origine-----
>> De : Bev Christian [mailto:[log in to unmask]] Envoyé : May-21-10 4:15
>> PM À : [log in to unmask] Objet : Re: [TN] RoHS compliance of stainless
>> stell
>>
>> Ioan,
>> Here are my answers to your questions below.
>>
>> 1) Can Stainless Steel be blindly considered RoHS compliant? Otherwise said, is there any SS hardware that could have any of the buggers (mainly Cd or Cr6)?
>> All stainless steels (assuming they are not coated - no reason why they would be, since they are inherently not prone to rust) would pass for Cr(VI) content.
>> BULK stainless steel does not contain lead and even if it did it could use the 0.3% by weight Pb exemption. However, see what I pulled off of the Health Canada website.
>>
>> "Health Canada warns Canadians about potential lead exposure from
>> stainless steel rum flasksWarning
>> 2003-18
>> April 10, 2003
>>
>> OTTAWA - Health Canada is warning Canadians that use of certain stainless steel liquor flasks may pose a lead exposure risk. The seams and the spout of the flasks in question were fastened together with solder that contains a high proportion of lead. Tests carried out by the Société des alcools du Québec (SAQ) on one brand of flask showed that, within 24 hours, hazardous levels of lead may leach out of the solder into liquid contained in the flasks. Therefore, anyone who drinks liquor or other liquids stored in the flasks for even short periods of time may be at risk of ingesting lead, particularly if the liquid is acidic.
>>
>> Health Canada has information that gift sets containing these stainless steel flasks which may pose a lead exposure hazard were sold from 1999 to 2003 in provincial or territorial retail liquor outlets across Canada. Flasks sold in the gift sets were approximately 6 oz in size and may be wrapped with leather. Provincial and territorial liquor control boards have issued recalls for two Appleton Estate gift sets, each containing a 375-ml bottle of rum, a Bacardi White Rum gift set, and the Wiser's De Luxe Canadian Whisky gift set. Consumers are advised to contact their local retail liquor outlet for specific product recall, return and reimbursement information.
>>
>> There is no lead exposure risk associated with drinking the bottled rum, whisky or other liquor included in the gift sets, provided that the liquors were not stored in the accompanying metal flask.
>>
>> Although no incidents of lead poisoning following use of these flasks have been reported to date, Health Canada is advising Canadians who may have one of these flasks in their possession to stop using it immediately.
>>
>> Lead is a toxic heavy metal. It can produce harmful effects on human health even at low levels of exposure. If you suspect lead poisoning from use of one of these flasks, contact your family physician who can order a blood test to measure your blood lead level.
>>
>> Health Canada is investigating the import and sale of this type of liquor flask on the Canadian marketplace and will issue an update to this warning if necessary."
>>
>>
>>
>>
>>
>> 2) Also, could some SS fall under the Pb exemption for machining?
>> See my answer above
>>
>>    3) And finally, some SS alloys are magnetic, some other aren't. Can SS hardware used in our industry be magnetic?
>> No clue about this one.
>>
>> Bev
>> RIM
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>> unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>> archives of previous posts at: http://listserv.ipc.org/archives Please
>> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at
>> [log in to unmask] or 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>> unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>> archives of previous posts at: http://listserv.ipc.org/archives Please
>> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at
>> [log in to unmask] or 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>> ---------------------------------------------------------------------
>> This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>> unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>> archives of previous posts at: http://listserv.ipc.org/archives Please
>> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at
>> [log in to unmask] or 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>> unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>> archives of previous posts at: http://listserv.ipc.org/archives Please
>> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at
>> [log in to unmask] or 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>>
>>      
> --
> Eric Christison Msc
> Mechanical Engineer
> Consumer&   Micro group
> Imaging Division
>
> STMicroelectronics (R&D) Ltd
> 33 Pinkhill
> Edinburgh EH12 7BF
> United Kingdom
>
> Tel:	+44 (0)131 336 6165
> Fax:	+ 44 (0)131 336 6001
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email
>
>    

-- 
Eric Christison Msc
Mechanical Engineer
Consumer&  Micro group
Imaging Division

STMicroelectronics (R&D) Ltd
33 Pinkhill
Edinburgh EH12 7BF
United Kingdom

Tel:	+44 (0)131 336 6165
Fax:	+ 44 (0)131 336 6001




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2