Hi Joe,
Unfortunately, a natural outcome of a proper reflow profile has become a
parameter to be aimed at. TAL is NOT a proper reflow parameter, and assures in and
of itself not good wetting and metallurgical bonding.
Adequate solder joint quality is assured with achieving Liquidus+20 C for 5
seconds at the slowest heating solder joint in the assembly. So whatever the
Liquidus temperature is for your solder alloy +20 for 5 seconds. For eutectic
SnPb that means 203C for 5 seconds at the slowest heating solder joint, which of
course means everything else on the assembly will see higher peak
temperatures for longer times [except for vapor phase, of course].
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
**************
Start the year off right. Easy ways to stay in shape.
http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|