Absolutely!
-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Bhanu Sood
Sent: Monday, January 6, 2020 11:10 AM
To: [log in to unmask]
Subject: Re: [TN] storage life of PCB microsection mold
And the microsectioned/prepped surfaces are protected from internal and external contamination.
> On Jan 6, 2020, at 11:44 AM, Stadem, Richard D <[log in to unmask]> wrote:
>
> I would assume it is just about forever as long as it was potted within the shelf-live and pot life of the mold potting material.
>
>
> -----Original Message-----
> From: TechNet <[log in to unmask]> On Behalf Of R Saravanan
> Sent: Monday, January 6, 2020 10:16 AM
> To: [log in to unmask]
> Subject: [TN] storage life of PCB microsection mold
>
> Dear all,
>
> What is the storage life of the pcb microsection mold . How long we can preserve.
>
> I am using long curing resin.
>
> R.Saravanan
|
|
|