TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Franklin D Asbell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Date:
Fri, 8 Sep 2006 07:00:17 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (202 lines)
I am curious where that is documented? I am aware DSCC has a 'preference'
but fir it actually be "not allowed" would mean 100's of drawings being
noncompliant. That seems unlikely.

Also, the supplier (board shop) would need to be qualified to MIL-PRF-31032
'before' they could build to the same specification, it is not a customer
driven transition.

Interestingly enough many companies are transitioning from 55110 to IPC 6012
instead of 31032.

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of - Bogert
Sent: Friday, September 08, 2006 4:02 AM
To: [log in to unmask]
Subject: Re: [TN] MIL-P-55110

Calling out a revision level of any military specification on a drawing is
not allowed by the DoD drawing requirements.  Also, folks should ask their
customers to allow them to transition to MIL-PRF-31032 in lieu of 55110.
This will help support more readily acceptance of the new specification, its
slash sheets and the QML for the spec.
  ----- Original Message -----
  From: James<mailto:[log in to unmask]>
  To: [log in to unmask]<mailto:[log in to unmask]>
  Sent: Thursday, September 07, 2006 7:59 PM
  Subject: Re: [TN] MIL-P-55110


  Mil-P-55110c can be built to and DESC does support this Rev and all
  subsequent revisions until it was superseded by Mil-PRF-31032. Any
  Revision call out is frowned on by DESC but not outlawed. Generally IPC
  specs are more frequently specified but as a Mil-PRF-31032 certified
  manufacturer I tend to lean towards the Mil spec. (which references many
  IPC specs).
  Unlike 55110, Mil-31032 requires manufacturers to build and submit for
  testing the highest technology build they want to be certified for. The
  is what differentiates it from the old 55110 and IPC 6012.
  To certify to IPC one just needs to build what is ordered and then test
  and retain. For 55110 one builds a 10 lyr qualification sample and then
  can build and test and retain. This 10 lyr sample opens the manufacturer
  up to build ANY 55110 technology.
  With 31032 one must submit a qualification test vehicle with the amount
  of layer and technology that represents the highest technology desired.
  So if one submits a 10 layer than that is the technology they are
  certified to.

  James
  [log in to unmask]<mailto:[log in to unmask]>

  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]] On Behalf Of Brad Saunders
  Sent: Thursday, September 07, 2006 3:49 PM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: Re: [TN] MIL-P-55110

  Hello Joe,
  Long, long time no see.  Trust all is well.
  I love the term "What does the Contract say?"  If your Customer is
  calling out 55110, then shame on them for calling out a revision.  Part
  requirements CAN'T call out rev: MIL-101.  [Approach politely]  You can
  actually go to them on that with full up DESC support.  I do full up
  55110, 31032 and or 6012; no problem.  The MIL versions are more work
  relative to reporting -globally, not part number specific.  We continue
  to submit monthly most challenging builds for 55110 and continually
  update 31032 (more than monthly) to ensure compliance to letter of the
  law (literally).  The 6012 Customers with failsafe environments get the
  same product; actually more stringent... especially the Class 3 and the
  Class 3A.
  As a Consumer that owns a half dozen computers and family in the Armed
  Services, all the specs are great.
  Yes, I would vote to see 55110 (and 50884) go away; however they DO have
  their place.  The time to argue part compliance to appropriate
  specification is before parts are in hand.  I trust the other fellow is
  back from vacation and the issue is at his feet.
  The MIL-PRF-55110 and the MIL-PRF-3102 and IPC-6012 are all alive well;
  I love these gosh darn PCBs... or is that pwbs.
  Brad
  603.234.2956
    ----- Original Message -----
    From: Kane, Joseph E (US
SSA)<mailto:[log in to unmask]<mailto:[log in to unmask]>>
    To:
[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:TechNet
@IPC.ORG>>
    Sent: Thursday, July 27, 2006 9:12 AM
    Subject: [TN] MIL-P-55110


    Our PWB expert is out on vacation, and I'm being drawn
    into a discussion with a customer about 55110C.

    We've moved to 6011/6012 for rigid boards, but I'm not sure
    exactly how we've documented or justified this change.

    My understanding is that the Mil spec has changed
    into a PRF, currently at Rev. G, and it's a practical
    impossibility to comply with 55110C because DSCC has
    gotten out of the business of administering the requirements.

    It would be great if I could show the customer a cancellation
    notice for 55110 that points to the IPC specs, but I can't
    seem to find one.

    Can anyone illuminate the trail please?

    Joe Kane
    BAE Systems
    Johnson City NY

    ---------------------------------------------------
    Technet Mail List provided as a service by IPC using LISTSERV 1.8e
    To unsubscribe, send a message to

[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:LIST
[log in to unmask]>> with following text in
    the BODY (NOT the subject field): SIGNOFF Technet
    To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:List
[log in to unmask]>>: SET Technet NOMAIL or (MAIL)
    To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:List
[log in to unmask]>>: SET Technet Digest
    Search the archives of previous posts at:

http://listserv.ipc.org/archives<http://listserv.ipc.org/archives<http://lis
tserv.ipc.org/archives<http://listserv.ipc.org/archives>>
    Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont<htt
p://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont>
  entpage.asp?Pageid=4.3.16> for additional information, or contact Keach
  Sasamori at
[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:sasako@ipc
.org>> or 847-615-7100
  ext.2815
    -----------------------------------------------------

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
  unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]>
with following text in
  the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
  (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET
  Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
  posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET
Technet Digest Search the
  archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives> Please
  visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentp
age.asp?Pageid=4.3.16> for
  additional information, or contact Keach Sasamori at
[log in to unmask]<mailto:[log in to unmask]> or
  847-615-7100 ext.2815
  -----------------------------------------------------

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentp
age.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori
at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
  -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2