Hi TN crickets (as to all the noise of underfill and coating)
Our production want send back 10 kilometers of single power cords. Insulator
is a single layer of Polyolefin. Now, when we crimp or solder these wires,
the following happens: when bending and gathering wires into bundles for
strapping and fixing them to chassis, the Polyolefn begins to withdraw from
the connectors or single contact pin. It creeps a few millimeters and I
think that won't have any kind of negative impact on electrical performance
or reliability or what so everm The amount of withdrawal in our company std
is set to be maximum one halv of the electrical wire diameterm. I found this
being a weird requirment, because IPC says 3 times the diameter.
1) So, what do you think, is a little withdrawal of the Polyolefin insulator
anything to bother about?
2) Do you know of a real good paper describing all about crimping . Molex,
T&B and some others had, but covers only what makes money.
Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|