TECHNET Archives

March 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 30 Mar 2010 09:26:49 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (78 lines)
Sealant based on my understanding is to fill a gap that may cause the ingress of harmful species; you need to know what are the two solid surfaces formed gap in between, how large the gap, what you try to protect with and for how long (assume you are not talking about infinity).  And assume you provide a good selection that will keep the gap filled sufficiently during the life of the unit under full operation environment (not just some op environment). Encap, goes on top of something, your device, solder leads, for ex.   The function is to provide intend support but not impede its function, hopefully enhance it.  For example, encap on globtop, block UV, provide support for wirebond, enhance thermal properties if you select filler properly.  Hopefully, it made a bit clear.  My 1.96 cent.  
--------------------------
Sent using BlackBerry


----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Tue Mar 30 08:54:03 2010
Subject: Re: [TN] Low Outgassing, Black Sealant / Underfill

Thank you, everyone, for the broad wealth of answers.  I now have a few options to run-down, so thanks to all.

Joyce, you made a comment that prompts some thoughts - that encapsulants and sealants are two different things?  I've considered that adhesives and sealants are different animals, and I understand that a sealant might not provide the structural support that an adhesive might, or an that an adhesive might not provide the moisture resistance a sealant might, but how do you consider that encapsulants and sealants vary?  Is it simply a difference in viscosity, whereas an encapsulant might be thinner than a sealant and flow around / under items whereas as sealant would be thicker and allow sealing over gaps, holes, or around components?  Would an underfill be considered more an encapsulant or a sealant?

Also, can anyone point out some background reading (papers) discussing when to underfill vs when to seal (or encapsulate)?

Thanks!



Kevin Glidden
Manufacturing Engineer
Astronics Luminescent Systems Inc.<http://www.astronics.com>
4 Lucent Drive
Lebanon, NH 03766
(603) 643-7766 x3152
________________________________
From: Glidden, Kevin
Sent: Monday, March 29, 2010 8:25 AM
To: 'TechNet E-Mail Forum'
Subject: Low Outgassing, Black Sealant / Underfill

Good Morning, and Happy Monday.

A couple of questions for anyone:

We have a lighting application where we are getting light reflection off two specific solder joints (we're so lucky to still use Sn63Pb37 they are just TOO shiny!), so I am looking for a method to cover those joints with a black (or dark gray) sealant.  This would need to be a low out-gassing material.  Does anyone know of any such material?  Is there such a thing as black pigmented conformal coating?

The second question would be for this same product.  I also have a need to seal around the base of some LEDs to prevent moisture ingress to the bottom only terminations.  Would perimeter sealing be sufficient?  How does one determine when they need to underfill vs perimeter seal?

Thanks!

Kevin Glidden

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2