TECHNET Archives

October 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Richard Haynes <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 28 Oct 1998 16:14:35 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (62 lines)
Josh,
Is the oxide copper oxides?
Richard

-----Original Message-----
From: [log in to unmask] <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Wednesday, October 28, 1998 2:40 PM
Subject: [TN] Oxide process controls


>We use oxide weight gain as a process control on our oxide line.  Recently,
it
>has been suggested that I consider using oxide peel strength tests as some
>sort of process indicator.  It has also been suggested that SEM's of the
oxide
>surface would be helpful in some way.
>
>I have always thought that SEM's were good for looking at oxide growth
>structure, but not for thickness or anything else.  I have the following
>questions:
>
>1.  Is anyone using SEM's of oxide surface for a regular process
>control/indicator?  What are you looking for in a SEM?
>
>2.  What peel strength should I expect to see from a non-reduced oxide in a
>polyimide application?  I've always thought that anything over 1 lb/inch
was
>good.  Is there some industry spec or standard for polyimide peels (oxide)?
>
>Thanks,
>
>Josh
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2