TECHNET Archives

September 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"<Rudy Sedlak>" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Sat, 16 Sep 2000 09:31:05 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (33 lines)
Howard:

I assume that the Copper whisker is against the laminate, not above it?
If that is the case, it is almost certainly caused by incomplete etching.
And if that is the case, the problem is almost certainly not caused by the
etching department.
My guess is that you are stripping photoresist using straight Caustic Soda.
(Most common strip chemistry in Taiwan)  If that is the case, the boards
probably tarnish badly in the stripper.
Tarnish on the Copper can interfere with (slow down) etching by the
ammoniacal type etchants used for etching outerlayers.
Figure out how to get panels with no tarnish to etcher, and you probably have
solved the problem.

Regards,

Rudy Sedlak
RD Chemical Company

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2