Contact your local Dow Corning rep., they have a product 'OS20
fluid' that can disolve cured RTV.
I have used it with good results. It requires 12-24 hours min. of
soak time.


Date sent:              Fri, 5 Nov 1999 21:06:49 EST
Send reply to:          "TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
From:                   Rudy Sedlak <[log in to unmask]>
Subject:                Re: [TN] Dissolution of cured RTV
Originally to:          [log in to unmask]
To:                     [log in to unmask]

It is POSSIBLE, although unlikely, that hot caustic soda, for a LONG period
my dissolve cured RTV, other than that, I suspect you are out of luck.

When you talk about a cured polymer, it needs more than a just a solvent to
dissolve it, you must actually break the bonds of the polymer, and destroy
it, and RTV is some tough stuff.

Regards,

Rudy Sedlak
RD Chemical Company

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2